TAURUS S/S TIG ROD 316L-2.4MM (5Kg)

R1399,00

SKU: 316L-2.4-T Category: Tag:

TAURUS TIG 316L rod is used for molybdenum-bearing austenitic stainless steels with 1.5- 3 % molybdenum. Type 316/316L steels are widely used for its good resistance to pitting, many acids and general corrosion.

WELDING POSITIONS
• Down hand

• Horizontal flat

• Horizontal vertical

• Vertical up

• Overhead

CLASSIFICATIONS
AWS A5.9 ER316L
EN ISO 14343-A G/W 19 12 3 L
EN ISO 14343-B SS 316L

COMPOSITION %
Carbon 0.03 Max
Manganese 1.0 – 2.5
Silicon 0.3 – 0.65
Sulphur 0.03 Max
Phosphorous 0.03 Max
Chromium 18 – 20
Nickel 11 – 14
Molybdenum 2 – 3
Ferrite number 3 – 10
MECHANICAL PROPERTIES AS WELDED
Tensile strength 605 MPa
0.2% Proof stress 465 MPa
Elongation on 4d 35 %
Impact energy at -130°C > 100 J
Impact energy at -196°C > 60 J
Scroll to Top