TAURUS MIG 316LSi is used for molybdenum-bearing austenitic stainless steels with 1.5 – 3 % molybdenum. Type 316/316L steels are widely used for their good resistance to pitting, many acids and general corrosion.
WELDING POSITIONS
• Downhand • Horizontal flat • Horizontal vertical • Vertical up • Overhead
CLASSIFICATIONS
AWS A5.9 ER316LSi
EN ISO 14343-A G/W 19 12 3 LSi
EN ISO 14343-B 316L Si
COMPOSITION | % |
Carbon | 0.01 |
Manganese | 1.7 |
Silicon | 0.8 |
Phosphorous | 0.015 |
Sulphur | 0.01 |
Chromium | 18.5 |
Nickel | 12.8 |
Molybdenum | 2.6 |
Copper | 0.15 |
Ferrite number | 6 |
MECHANICAL | AS WELDED |
Tensile strength | 570 MP |
0.2% Proof stress | 435 MPa |
Elongation on 4d | 42% |
Elongation on 5d | 40% |
Impact energy @ -130°C | < 70 J |
Impact energy @ -196°C | 30 – 60 J |